Jacob Scherer Posted October 23 Posted October 23 (edited) Hello everyone! I've been a longtime lurker on this forum since I discovered it in 2014, and I've been popping by for inspiration and advice a few times a year ever since. This place has been such a wealthspring of information, I'm excited to be contributing for the first time. My goal is partly to chronicle the process and partly to seek feedback on my future plans, since this is considerably more complex than the hot work I've normally done. My interest in bladesmithing comes primarily from an interest in historical combat. I do both archery and historical fencing, so the ability to make and modify my own gear has always been a benefit. I've done a considerable amount of hot work, and a considerable amount of grinding, reprofiling, sharpening, polishing, etc...but mainly in the context of re-hilting and re-grinding blades that have broken, come loose, or otherwise needed to be modified (sometimes extensively). I've forged from scratch and quenched a handful of knives, but the bulk of my experience lies elsewhere. And that's why this project stands out: there is a serious dearth of reproduction yari on the market, and I have the desperate urge to test one against various forms of armor. The obvious course of action is to simply make one. The yari fascinates me because it seems to have a very strange set of features (to an eye accustomed to European arms). On the one hand, they're thick, typically rather narrow, and triangular in profile, suggesting they are designed to pierce armor. And yet, they have very rounded points (compared to many European polearms designed to pierce armor), AND my understanding is that they tend to be heat-treated at a lower temperature than you would expect for a weapon that takes a lot of sudden impacts, implying the makers prioritized a very hard edge over toughness. How to interpret this collection of details? Most tests of European spike-based weapons that I've seen or performed indicate that they mainly cause mail rings to fail by wedging them open and bursting them, either at the rivet or near one of the edges. That, to me, implies that the points on, say, a halberd or a rondel dagger are mainly targeting the tensile strength of the ring, rather than attempting to shear through them. My initial impression of the yari is that the tips are too wide to wedge themselves that deeply into most mail rings. In contrast to a rondel dagger, very little of the point would be sticking out the back before a ring is compromised. Instead, the very hard edges and sloped tip lead me to believe that the intention is to actually, properly CUT the wire, since most mail was made of iron or mild steel. My curiosity likely would've stopped if I could look up a video of someone actually testing a yari on some armor, but I haven't been able to find any good ones. So, here I am. I started with 3/4 inch mild steel round bar (I'll explain the steel decision later), and got here: This was my first time forging bevels (I usually just grind them in), and I think they turned out ok. They're not nearly as steep as they need to be, but I feared that a miss hit could reduce the thickness by too much, and I'm trying to keep this sucker as thick as possible (10mm+ throughout). 550g at this stage. The tip came out a little funky, but I could fix that in grinding. Speaking of which: This is where we landed with the profile established and the tang ground to size. The finished length has the blade (counting everything above the tang as the blade, not just the edged portion) at 7.5 inches and a tang length of 10.5 inches. That appears to be on the more modest side for yari heads, but I balk at the notion of fitting a 20 inch tang into a spear shaft. Hard pass. From there, I moved on to the bevels, which ended up here: The midrib is still a bit wavy, but I can fix that once the bevels on this side actually meet the flat on the other side (not pictured, my bad). I don't even know what the edge angle will be on this thing, but...robust. I haven't touched the kerakubi (the little neck between the blade and the tang), because I need to figure out how many facets I want and how much narrower I can make it while sacrificing as little structural integrity as possible. It's still a full .75 inches above the tang. 450g at this stage. Now, onto the question of heat treatment: I could not, for the life of me, find reasonably priced 3/4 inch round bar in any knife-worthy steel, especially since all my research indicates that yari would've had very high-carbon edges like any other nihonto. Plus, it needs to be differentially hardened through claying, and that means ideally I would emerge with a hamon.... Then, it occured to me: carburizing! I was unaware, until watching this video, that you could get a carburized layer that deep in a piece of steel. 3-4mm of carbon penetration would be enough to give me my hard edge, with the added benefit that it would compliment the differential hardening by offering a softer core steel, as well. As a final note, I'm locked into water quenching this blade. I do all my metalwork at a local makerspace, and they don't allow oil quenching in the building (fire hazard). Plus, I do think there's good reason to go for water. I WOULD like a hamon if possible, and with the thick cross section this blade is going to have, I'm thinking a more aggressive quench might be called for anyways. Plus, the carburization process should leave me with a relatively simple high carbon steel skin, right? Somewhere in the 1070-1095 range? I saw a wonderful comment on here years ago detailing how the poster got near-flawless results by quenching in brine made from distilled water for 3-4 seconds, straightening, then going right away into a 450-500 degree oven. Supposedly, that would let the temperatures in the steel even out before martensite forms, then let it air cool so that the martensite formation causes fewer internal stresses (?). Unfortunately, he didn't specify the time the blade should spend in the oven, so if anyone could shed some light on this process, I would be grateful. So...what am I missing? What sort of carbon content would I be looking at if I packed the blade with charcoal and salt paste, sealed it with clay, and fired it at 1700-1800F for 1.5 hours? Can you even get a hamon on carburized steel? Is the quench described above a viable method, or should I just go the traditional route of praying I don't hear a ping? What are my blind spots? I know this is an ambitious step for someone who doesn't do a great deal of hot work or heat treating, but I've always enjoyed throwing myself into the deep end, and I started this project putting its success at a coin toss. I've learned a great deal by breaking things, so if this project turns out the same way, I won't be too put off, and hopefully others can learn from my folly. Thanks! Edited October 23 by Jacob Scherer Added weight after initial bevelling. 1
Alan Longmire Posted October 24 Posted October 24 That looks good, and is indeed ambitious! I just checked, and you're right, 3/4" round W-1 drill rod from MSC is $54 for a three foot bar. That's twice what I paid for it a couple of years ago. As for carburizing, doing it with plain charcoal isn't going to do much, and the salt is not a good idea. You don't want sodium or chlorine in your steel. The old way was to use leather and bone charcoal. Something about the calcium content improves the reaction, speeding it up substantially. Ric Furrer and Kevin Cashen did a lot of experimentation with this when they were playing with shear steel production a few years ago, Keven had some good videos explaining the process on his website. Dunno if they're still available. Anyway, if you did that, you could do the brine quench and straight into the oven. I don't think you'd get hamon, since you'd be carburizing the entire surface and thus case-hardening the whole thing. You might be able to carburize, let cool, then reheat and quench. The thickness of the center would be enough to keep the core from hardening fully, but I'd worry the carbon diffusion effect would mean the edges would no longer have enough carbon to harden at all. Which leads me to what I'd do... Case hardening with a modern case-hardening compound. The directions are on the tin, and vary by brand, but this one is typical and seems to be the most readily available: https://blacksmithsdepot.com/supplies/heat-treating.html/cherry-red-hardening-compound.html It's nontoxic, unlike some of the older compounds that used cyanide. I've used it and it works very well. The question is how deep a case will you get by traditional methods versus modern. The stuff I linked says 0.010", and I suspect the traditional way would be similar unless you go a couple of hours and get blister steel. I'll be thinking about this.
Jacob Scherer Posted October 25 Author Posted October 25 Thanks, Alan! 18 hours ago, Alan Longmire said: The old way was to use leather and bone charcoal. Something about the calcium content improves the reaction, speeding it up substantially. I looked it up, and it seems that calcium carbonate is one of the things that would speed up the reaction. 18 hours ago, Alan Longmire said: You might be able to carburize, let cool, then reheat and quench. The thickness of the center would be enough to keep the core from hardening fully, but I'd worry the carbon diffusion effect would mean the edges would no longer have enough carbon to harden at all. I hadn't even thought about this. I wonder how quickly that would happen at normalizing or austenitizing temperatures, compared to the 1700-1800 at which I'd do the actual carburizing. 18 hours ago, Alan Longmire said: The question is how deep a case will you get by traditional methods versus modern. The stuff I linked says 0.010", and I suspect the traditional way would be similar unless you go a couple of hours and get blister steel. You've made me curious enough to do a test. I mixed charcoal powder and flour (just as a binder) with some water to make a carbon-rich dough. For the calcium carbonate, I just ground up some antacid tablets and mixed them in, as well. I packed it around a few lengths of 3/8 inch mild steel round bar, baked them until dry, then sealed them with refractory cement (since I didn't have any clay on hand). I'll stick them in the gas forge at ~1800F for an hour. The first, I'll quench right out of the forge after knocking off the cover. The other, I'll clean off, normalize for 10 minutes/air cool, then quench at nonmagnetic--essentially treating it like a normal piece of steel. I'll break both, look at the grain size, and report back.
Jacob Scherer Posted October 25 Author Posted October 25 (edited) Made some more progress today. The grinding is largely finished, the shoulders are cut, and the shaft is in one piece. I laminated two halves together after rough-chiseling a space for the tang, then burned in the final fit (which worked like a charm). I officially did something dumb, which was forgetting to drill the holes for the mekugi peg BEFORE laminating the shaft, but oh well. I'll figure something out. I lost a bit of thickness trying to get the midrib right. The minimum thickness of the blade (excluding the very tip) was 10.1 mm before. Now it's 8.8. Oh well. Something tells me it'll survive. The thickness of the neck is 13.4 mm. The weight is now 360g. The next steps are 1) sand and polish, 2) figure out and subsequently employ whichever case hardening method will give me the thickest carbon steel layer, and 3) shape the shaft. It's 1.5 inches thick at the moment. Based on the originals I've seen, they all seem to taper toward the tip, so my initial plan is to go with ~1.25 inches for the bottom 2-3 feet, taper to 1 inch about 6 inches from the end of the shaft, then down to .75 inches to marry up neatly with the shoulders of the head. The 2-3 feet of the shaft nearest the head are going to be wrapped in rawhide (to prevent the tang from splitting the wood) and lacquered, so I'm not terribly worried about reducing the thickness to under an inch once the shaft reaches the tang. Edited October 25 by Jacob Scherer Forgot parenthesis; added weight measurement 2
Alan Longmire Posted October 25 Posted October 25 5 hours ago, Jacob Scherer said: I hadn't even thought about this. I wonder how quickly that would happen at normalizing or austenitizing temperatures, compared to the 1700-1800 at which I'd do the actual carburizing. I looked as well. Consensus seems to be ~ 10 microns/minute at austenitizing temps, exponentially faster at welding temps. Hopefully Jerrod will step in, I couldn't get the one table of carbon diffusion rates I have a link to to open. I'm glad you're experimenting!
Jacob Scherer Posted October 26 Author Posted October 26 Well, I definitely got results. What kind of results, I'm not sure. If someone with more experience in looking at steel cross-sections could chime in, I would appreciate it. I ended up cutting my initial carburization test short at 45 minutes, rather than an hour, in part because the gas forge at the makerspace kept sputtering/backfiring at lower gas pressures, so the minimum temperature it would hold reliably was more like 1900F, rather than 1700F. At any rate, one sample was quenched in water as soon as the initial carburization was finished. I broke open its envelope and took it straight to the quench. The other was broken out and allowed to air cool. Because of the forge issues last night, I couldn't exactly normalize it at anywhere close to a reasonable temperature, so all I did was take it back up to nonmagnetic in the induction forge and quench. Interestingly, the sample that went straight into the quench refused to break when I clamped it in the vise and bent it. It did spark like crazy when ground, though, and the surface cracked to a depth of about half a millimeter, so SOMETHING chemically significant happened. The one in the picture is the sample that was allowed to air cool then taken to nonmagnetic. If I'm reading this image correctly, there's a noticeable ring of finer-grained steel around the edge of the bar. If that's the carburized layer, like I think it is, then I measured it at about .02-.028 inches, which is pretty good for only 45 minutes in the forge. If I cook it for 1.5 hours, I may wind up with a full millimeter of carburization, which seems like it would be sufficient to give the spear edge some resistance to deformation. What do we think about the texture of that high carbon ring? If this were a normal piece of steel, I'd obviously be worried about grain size from holding it at 1900F+ for so long, but I'm unsure if the same rules apply in this case.
Alan Longmire Posted October 26 Posted October 26 That grain growth is why modern case hardening compounds work at lower temperatures instantly. If you can do a triple normalization on that one it might look pretty good without affecting the carbon distribution all that much. That center grain needs to be reduced as well. Large grain is not tough grain.
Jacob Scherer Posted October 26 Author Posted October 26 1 hour ago, Alan Longmire said: That grain growth is why modern case hardening compounds work at lower temperatures instantly. If you can do a triple normalization on that one it might look pretty good without affecting the carbon distribution all that much. That center grain needs to be reduced as well. Large grain is not tough grain. Sounds like a need to do another test with a longer carburization time and some normalization cycles, then. I'll make some test coupons in a triangular cross section like the spear blade to see what's happening at the edges, as well. I'll pick up some clay, too, so that I can make a better seal than with forge cement. Maybe play with the calcium carbonate ratios, as well. Any guess what kind of carbon % I might be dealing with? Also, thank you for all the feedback. I'm glad to have some guidance on this project.
Alan Longmire Posted October 26 Posted October 26 It's the squinty one-eyed guy leading the blind, but I try! Carburizing that way gets you a max of around 0.75-0.90 %. 1
Jacob Scherer Posted November 3 Author Posted November 3 Well, progress has been made! First things first, I prepared two test coupons to try out different normalization cycles and see how they impact the carbon steel layer resulting from carburization. The coupons were ground thinner on one side to give me some idea of how carbon migration might differ in different cross sections. Next, they were wrapped in carbon dough and baked until dry. Carbon dough consisted of: 80g charcoal powder, 30g flour (binder), 4 peppermint tums tablets (4g calcium carbonate). Yummy. These were wrapped in clay, dried again, cracks sealed with forge cement, then fired at 1950F for 1.5 hours. While that was going on, I tapered the spear shaft. Total weight of the spear as of now: 1300g. Total length: around 7.5 feet, maybe a bit more. Once the test coupons had been fired, they were allowed to cool in air. Both then went into the furnace to normalize. The first cycle lasted 15 minutes at 1650-1700F (I was having trouble keeping the temp constant at first). The first test coupon was then allowed to cool, brought to nonmagnetic, quenched, and broken. We did it, boys! That right there is a .05 inch high carbon layer, just shy of 1.5mm. I feel pretty happy about that. Much to my surprise, the grain size looked pretty good, too (in my relatively untrained opinion). The next test coupon was normalized twice more, once at 1600-1650 and once at 1520 or thereabouts. Both for 10 minutes, then left to air cool. It was, likewise, brought to nonmagnetic and quenched. And....is it just me, or do the grains look bigger? The carbon layer is roughly the same thickness, but the grain size looks larger to me. On the left is the once-normalized sample, on the right is the thrice-normalized sample. I definitely think the once-normalized sample has a tighter grain, but I can't really figure out why. At any rate, both are a step in the right direction over my previous tests, and I think 1.5mm of carbon steel is enough to work with. I think this is a workable method for hardening the spearhead. As always, comments, critiques, and advice are welcome. Thanks!
Brian Dougherty Posted November 3 Posted November 3 The grain may be caused by spending too much time at temperature. You don't want to soak at temp while normalizing. Just get it up to the transition temp and let it cool. I'd bet your temps are a little too hot as well. Once you see the shadows moving in the steel, you're done and should let it cool off. 1 -Brian
Alan Longmire Posted November 3 Posted November 3 What Brian said. Soak times are for complex alloys, simple carbon steels just grow grain. The furnace is great for doing the carburizing, but you'll want a forge for normalizing. Just rock it back and forth across the transition a few times, that grain will shrink to invisibility. Your first sample grain is way too big, the second is completely unacceptable. But yay on the hard case! Experiment successful, now you just need to rethink your normalizing routine.
Jacob Scherer Posted November 3 Author Posted November 3 (edited) I somehow went all this time without realizing that soak times for simple carbon steels aren't a thing. Well, my job just got a whole lot easier! Thanks, guys. 51 minutes ago, Alan Longmire said: The furnace is great for doing the carburizing, but you'll want a forge for normalizing. I should clarify: all of this is being done in a propane forge. I tend to use "furnace" in a generic sense to mean "box containing fire," a habit I should work to break when writing on here. I've been using a type K thermocouple to tell what temperature I'm at, but since I just need to bring the steel up to critical then let it cool, I might try the melting salt trick. I seem to remember that table salt melts at virtually the exact critical temperature of 10xx series steels. Edited November 3 by Jacob Scherer forgot the word "critical"
Alan Longmire Posted November 3 Posted November 3 Okay, now we're cooking! Find yourself some steel pipe or tube that can hold the yari. Weld one end of the tube shut. After carburizing, let the steel cool, then remove all the gunk to leave clean steel. Put the tube in the preheated forge and let it heat until it's glowing evenly at around 1500-1600F. Throw a little wood or charcoal, like a 1" x 1/2" chunk, into the tube and push it to the back of the closed end. That will make a reducing atmosphere in there, so your steel won't scale. Now put the steel in the tube. As it gets into the red range, watch it carefully. Being protected from the flame front in the forge, you will be able to see when the edges turn orange. As they do, you'll notice what looks like a dark line, then a shadow swirling under the surface of the steel. That is the atoms absorbing photons during the crystalline phase change from body-centered cubic to face-centered cubic structure, aka critical temperature. As soon as the shadows have disappeared and the whole thing is bright orange, pull it out and let cool in still air. If it's dimly-lit enough in the shop, you will see the reverse effect: a bright line will move from the edges inwards as the crystalline phase shifts back. Congratulations, you have now normalized it once! Let cool to black in still air, and repeat twice. This will give you good machinability and the finest grain structure you'll get without entering the realm of diminishing returns. The swirling shadow phenomenon is called decalescence. It's the single most important thing to observe when heat-treating simple and low-alloy steels. When you have it, you need no further temperature measurements. 1095? It works every time. 5160? Yep. W-1? absolutely. 1045? Even that. 15n20? Works fine. 52100? Excellent. O-1? yeah, but that you do need to soak a minute or two to get the best performance. Stainless? Nope. Not at all, sorry. Too much other stuff in there to rely on the phase change. And I'll bet you didn't think crystallography and quantum physics had any place in bladesmithing. 1
Recommended Posts
Create an account or sign in to comment
You need to be a member in order to leave a comment
Create an account
Sign up for a new account in our community. It's easy!
Register a new accountSign in
Already have an account? Sign in here.
Sign In Now